热腐蚀

  • 网络Hot corrosion
热腐蚀热腐蚀
  1. 激光熔敷Co基合金的组织及涂盐热腐蚀性能

    Study on the microstructure and salt-coating hot corrosion resistance of laser cladding Co-base alloy

  2. (Al,Mn)3Ti-2V金属间化合物的热腐蚀研究

    Investigation of hot corrosion of ( al , mn ) _3ti - 2V Intermetallics

  3. 高Cr含量镍基高温合金热腐蚀行为研究&I.实验研究

    Hot corrosion behavior of Ni-based superalloy with high Cr contents - part 1.experimental study

  4. Mn和V对TiAl合金热腐蚀的影响

    Effect of Mn and V on hot corrosion of TiAl Alloy

  5. 发现Ni3Al-0.2B耐熔盐热腐蚀能力极差,硫化-氧化是腐蚀破坏的主要原因。

    The hot corrosion resistance of Ni_3Al-0.2B is quite bad , and the sulphidation-oxidation is responsible for corrosion damage .

  6. 运用SEM、XRD、EDS等方法分析了原始涂层和经过腐蚀后涂层的微观形貌,初步探讨了高温下氧化、涂盐热腐蚀及硫化腐蚀机理。

    Mechanisms of high-temperature oxidation corrosion , salt coated corrosion and sulfidation corrosion were discussed .

  7. TiAl金属间化合物在熔融碳酸盐中的热腐蚀行为

    Hot corrosion behavior of TiAl intermetallics in the Molten Carbonates

  8. TiC基金属陶瓷耐高温熔盐热腐蚀性能的研究

    Study on hot-corrosion resistance of TiC-based cermet

  9. 渗铝钢在Na2SO4-V2O5熔盐体系中的热腐蚀行为

    Hot Corrosion Behavior of Aluminized Steel in Na_2SO_4-V_2O_5 Molten Salt System

  10. Al-Si涂层在900℃硫酸盐中的热腐蚀行为

    Hot corrosion behavior of an Al-Si coating in presence of molten sulfate film at 900 ℃

  11. FeCrAl涂层低温热腐蚀形成疏松的Fe2O3是其腐蚀的主要原因。

    The loose Fe_2O_3 formed in low-temperature hot corrosion of FeCrAl coating is the main reason of the corrosion .

  12. 预氧化Fe-Cr合金在KCl盐膜下的热腐蚀行为研究

    Study of Hot Corrosion Behaviors of Pre-oxidized Fe-Cr Alloys under KCl Deposits

  13. 熔融NaCl-(Na,K)2SO4引起的Fe-Cr合金的热腐蚀

    Molten nacl - ( na , k ) _2so_4 induced hot corrosion of Fe-Cr alloys

  14. 用水热腐蚀法,通过改变腐蚀液中Fe(NO3)3的浓度,制备多孔硅样品。

    Three porous silicon ( PS ) are prepared by Hydrothermal Etching with different Fe ( NO3 ) 3 solution concentration .

  15. Na2SO4沉积引起的Fe&10Cr合金在700℃的热腐蚀

    Na_2so_4 deposits induced hot corrosion of Fe-10 Cr alloy at 700 ℃

  16. 由Na2SO4沉积引起的高温合金B&1900在中温下的热腐蚀

    Na_2so_4 induced hot corrosion of b - 1900 superalloy at intermediate temperatures

  17. 合金元素对Ti3Al基金属间化合物热腐蚀性能的影响

    Effects of alloying elements on hot corrosion resistance of ti_3al intermetallic compound

  18. Fe3Al合金堆焊层的高温热腐蚀行为研究

    Hot Corrosion Behavior of Fe_3Al Overlay at High Temperatures

  19. 利用电化学方法、热腐蚀试验等研究了GD型钢纤维在工业磷酸中的腐蚀行为。

    The erosion of GD type steel fibre in industrial phosph-acid has been tested by the electrochemistry and thermal etching testing .

  20. 二元硫酸盐Na2SO4-K2SO4沉积引起的Fe-Al合金的低温热腐蚀

    Low temperature hot corrosion of Fe-Al alloys induced by na_2so_4-k_2so_4 deposit

  21. 表面有Na2SO4沉积时铁基合金的低温热腐蚀行为

    Low temperature hot corrosion behavior of iron base alloys in the presence of na_2so_4 deposit

  22. Mn和V对TiAl金属间化合物在900℃(Na,K)2SO4熔盐中热腐蚀行为的影响有所不同。

    The effect of Mn and V on hot corrosion of TiAl in ( Na , K ) 2SO4 melt at 900 ℃ has been investigated .

  23. FeCrAl合金涂层抗高温氧化及热腐蚀性能研究

    Performance of High Temperature Oxidation and Hot Corrosion Resistance of FeCrAl Alloy Coating

  24. Pd-Ni-Al涂层的循环氧化和在Na2SO4熔盐中的热腐蚀行为

    Cyclic oxidation and hot corrosion behavior of Pd-Ni-Al coatings

  25. 利用热腐蚀法制备出用于环境扫描电镜(ESEM)研究反转电畴结构的样品。

    The samples used for examining the reversal domain with ESEM were prepared by heat erosion .

  26. Na2SO4-MgSO4-CaSO4沉积引起的铁基合金的热腐蚀Ⅰ.在空气中的腐蚀

    Na_2so_4-mgso_4-caso_4 induced hot corrosion of iron base alloys ⅰ . corrosion behaviour in air

  27. 本文中,我们使用水热腐蚀法制备了一系列铁钝化多孔硅(Ironpassivatedporoussilicon,IPS),研究其光致发光(Photoluminescence,PL)和光电导性质,并探讨其内在的机制。

    So in this thesis , we prepared a series of iron-passivated porous silicon ( IPS ), and studied their photoluminescence properties and photoconductivity characteristics , the possible mechanisms were also discussed .

  28. 试验结果表明,在本试验的参数条件下,试验表面的破坏是以石英砂的高温冲蚀磨损为主,SO2气氛的热腐蚀作用不明显。

    The experimental results show that the wastage of sample surface is mainly caused by erosion of sand at high temperature and hot corrosion of SO 2 atmosphere is not serious .

  29. 通过SEM,XRD,EDS,盐腐蚀试验,热腐蚀试验和电化学测试等研究了锌铝铬膜的防腐蚀性能与机理。

    The anti-corrosion characteristics and mechanism of zinc-aluminum-chromium coating were studied by tests of salt immersion , salt spray and heat treatment test , and by examinations of electro-chemical impedance spectra , SEM , XRD and EDS.

  30. Pt-Al涂层在两种熔盐中的高温热腐蚀行为

    Hot corrosion behavior of Pt Al coating in molten sulphate or mixed salts