焦炭反应后强度
- 网络csr;Coke Strength after Reaction
-
焦炭反应后强度(CSR)提高了6.8~8.63个百分点;
The CSR of the coke raised by 6.80 ~ 8.63 percent .
-
以焦炭反应后强度指标为依据操作2500m~3高炉的生产实践
Production practice of operating 2 500 m 3 BF based on the strength of coke gasification reaction
-
碱金属对焦炭反应性和反应后强度的影响
Alkalis affect both reactivity and strength after reaction coke
-
焦炭反应性及反应后强度预测模型研究与分析焦炭气化反应及对其强度的影响
Model prediction for CRI and CSR study on gasification of coke and its influence on coke strength
-
以高炉顶部加入粒煤为背景,研究无烟煤的加入量对不同焦炭反应性和反应后强度的影响。
Discusses the addition of anthracite and the influence of anthracite on the reactivity and the strength after reaction of different coke .
-
沪市A股过度反应和反应不足的实证研究焦炭反应性及反应后强度实验中注意事项
Empirical Study on Overreaction and Underreaction of Shanghai Stock Exchange s A Shares ; The points of attention in detection of CRI and CSR of coke
-
本文首先研究了武钢炼焦生产用煤的煤质、灰分组成和催化指数,并进行了配煤炼焦试验和焦炭反应性和反应后强度的测定;
In the paper , firstly , coal properties for coking in WISCO , ash composition and mineral catalytic index are researched and coking experimentation in laboratory coke-oven and CRI and CSR determination are carried out ;
-
生产使用结果表明,配用澳大利亚炼焦煤后焦炭灰分、硫分降低,并显著地改善了焦炭的反应后强度。
The result showing that the contents of ash and S are lower when using BHP , At the same time , BHP improved the intensity of the coke prominently .
-
作者通过焦炭的浸碱试验,阐述了碱金属对焦炭反应性和反应后强度的影响,认为碱金属加速了焦炭的气化反应。
This paper explains the ways alkalis affects both reactivity and strength after reaction coke through the experiment of coke dip alkalis .
-
模拟焦化厂熄焦过程和焦炭转运过程,用ZBS溶液对焦炭进行处理,通过系列实验重点研究了ZBS添加剂对焦炭反应性、反应后强度的影响。
The coke was first sprayed with the ZBS solution under simulating coke quenching process and cool-coke transport process at coke plant . The influence of the ZBS additive on coke property such as CRI and CSR has been analyzed and discussed by means of a series of experiments .
-
碱金属化合物对焦炭的溶损和铁矿石的还原有催化作用:当K2O含量超过1.5%时,焦炭的反应性(CRI)提高23%左右,焦炭反应后的强度(CSR)约降低40%;
The alkali metals adhering to charges have a catalytic action on gasification reaction of coke ; When K_2O % is above 1.5 , the CRI of coke will be increased by 23 % and CSR will be decreased by 40 % .