利用XRD,TEM和EDX分析球磨后粉末的晶粒尺寸、晶格畸变、形貌、结构变化及颗粒成分变化。
The grain size , lattice deformation and morphology , of the component of particles after milled were analyzed by means of XRD , EDX and TEM .
-
同时,激光诱导晶格畸变可能使多孔硅由线性变为非线性光学材料,而且具有非常大的光致非线性吸收系数。
The laser-induced lattice deformation may result in the transformation of the porous silicon from a linear to a nonlinear optical material with a large laser-induced nonlinear optical absorption coefficient .
-
在煅烧以后,c轴伸长明显使原有的晶格畸变消失。
After calcination the lattice parameter c grows obviously and the old crystal lattice distortion disappears .
-
多孔硅层晶格畸变的X射线双晶衍射研究
Investigation of lattice deformation of porous silicon films by X-ray double crystal diffraction
-
C~+注入Si的晶格畸变
The Lattice Strain of C + Implanted in Si
-
Mn掺杂导致了显著的局部晶格畸变。
A local crystal structural distortion induced by Mn doping was found .
-
XRD分析结果还表明纳米ZnO中存在一定的晶格畸变现象。
Results of XRD show that there exists distortion of crystal lattice in nanocrystalline ZnO .
-
N(Z)的和图.金刚石的晶格畸变
Lattice Distortion in Diamonds
-
用XRD线形分析法表征TiC粉体中的镶嵌尺寸与晶格畸变
Crystallite Size and Lattice Distortion of TiC from X-ray Diffraction Line Profile Analysis
-
利用x射线衍射法对铜锌和铜锌铝系低压合成甲醇催化剂还原态的结晶铜和氧化锌晶格畸变进行测定。
The crystal copper and distorted zinc oxide lattice of reduced low-pressure synthetic catalyst of methanol are studied with XRD .
-
MgO的晶粒大小和晶格畸变与水化活性的关系
Relationship between Crystalline Size and Lattice Distortion of MgO and its Activity
-
Mg或Cd掺杂尖晶石型LiMn2O4的晶格畸变
Lattice distortion of Mg or Cd doped spinel LiMn_2O_4
-
PZT四方相区介电常数εr与晶格畸变关系的研究
Study on the relation between the dielectric properties and lattice distortions in PZT ferroelectric tetragonal phase region
-
纳米Ag粉体的晶格畸变
Lattice Distortion of Nano-Ag Powders
-
位错处存在晶格畸变,杂质易于在此处聚集,达到一定浓度就会抑制晶体在此处生长而形成V缺陷。
There were lattice distortions in the dislocations , impurities concentrated here easily , V defects appeared on the dislocation sites .
-
晶格畸变对KCl中FH(CN)~-的基态的影响
Influence of Crystal Lattic Distortion On the Ground State of F_H ( CN ) ̄ - in KCl
-
利用X射线双晶衍射方法,对从同一Si(111)基片上切割的两块样品,在不同电解电流密度下,腐蚀形成的多孔硅层相对于基体硅的晶格畸变进行了分析。
An investigation on the lattice deformation of porous silicon layer was completed by means of symmetric and asymmetric X-ray double crystal diffraction .
-
结果表明:影响铁素体球铁曲轴硬度的主要元素是硅,硅溶于铁素体(-αFe)形成置换固溶体,造成晶格畸变,引起硬度提高。
Silicon was the main element which dissolved into ferrite to form substitutional solid solution , and caused lattice distortion and increased hardness .
-
通过XRD及SEM分析,冲击波对HA团聚体粉末具有明显的均化与细化作用,并产生了一定程度的晶格畸变。
The grain size refinement , homogenization and dislocation of lattice in shocked HA powders were analyzed by XRD and SEM .
-
Al2O3∶Cu~(3+)晶体EPR参量及其晶格畸变研究
An Investigations of the EPR Parameters and the Lattice Distortion in Al_2O_3 ∶ Cu ~ ( 3 + ) Crystals
-
XRD结果显示:添加助磨剂六偏磷酸钠使晶粒尺寸减少和晶格畸变程度增大。
The XRD results indicated that adding sodium hexametaphosphate as grinding additive reduced the crystal size but increased the lattice distortion degree .
-
我们还研究了PT四方相区和立方相区介电常数与晶格畸变的关系。
We also study the relation between the dielectric constant and lattice distortion of the PT tetragonal and cubic phase region .
-
高能机械球磨引导的纳米TiO2晶格畸变和高压相
Lattice Distortion and the High Pressure Phase in Nanoparticles TiO_2 Induced by High Energy Mechanical Milling
-
计算晶格畸变应力e数据表明,Ti4+可能反掺入了表面稀土氧化物的晶格中。
The data of lattice distortion implied that Ti4 + could enter ( anti-dope ) into rare earth oxide that existed on the surface of titanium dioxide .
-
在αMg基体中存在着大量的大角度亚晶和较高密度的位错缠结以及较大程度的晶格畸变。
There exist a great mount of sub-crystal with big angle and dislocation tangles with high density as well as lattice distortion in α - Mg matrix .
-
适当的热退火能促使Fe颗粒生长,使晶格畸变减小,从而改善膜的微结构。
Appropriate annealing can improve the microstructure of the films due to the growth of Fe particles and the decrease of the distortion of the crystal lattice .
-
我们对PZT四方相区、角相区和混合相区介电常数与晶格畸变的关系进行了全面研究和探讨。
We comprehensively investigate and discuss the relation in the tetragonal , rhombohedral and coexistence phase region of PZT .
-
不同的基底与Fe薄膜的界面错配度不同,可改变薄膜晶体位向的分布,导致晶格畸变程度和晶粒尺寸的变化。
Various substrates induce different interfacial mismatch between the film and substrate , and result in the changes of lattice distortion degree , grain size and texture distribution .
-
YAG:V~(2+)激光材料晶格畸变及其EPR参量研究
Investigations of Lattice Distortion and EPR Parameters for YAG : V ~ ( 2 + ) Laser Crystal
-
采用X射线衍射、拉曼光谱、DTA和透射电镜对产品进行了表征,计算了常温下亚稳的四方氧化锆晶粒的晶格畸变率。
TEM , XRD , DTA and Raman spectrum were used to characterize the samples , and the crystal lattice distortion rate was also calculated .