Influence of Joining Strength of Si_3N_4 / S45C on Residual Stress
残余应力对Si3N4/S45C连接体强度的影响
-
The chemical composition , microstructure , fracture morphology and hardness of cracked S45C steel parts were tested and analyzed .
对淬火开裂的S45C钢零件进行了化学成分、金相组织、断口分析及硬度检测。
-
Simulation analysis shows that for the steel ( S45C ) wheel , the cooling rate is relatively small because of its big size .
模拟分析发现,45号钢车轮淬件尺寸较大,自身冷却速率较慢。
-
The efficiency of the present method is shown by comparing the numerical hardness results of S35C and S45C with experimental ones .
通过对S35C和S45C两种材料进行的解析和实验结果的比较,证明了解析法的正确性。
-
The three-dimensional temperature fields of a steel ( S45C ) wheel are calculated under different conditions , water quenching and water-oil quenching process .