The general corrosion rate of 316 is higher than 1 00mm / a. Pitting penetration rate is more than 1 5j ~ tm / h.
316的均匀腐蚀速度甚至高于100mm/a,孔蚀穿透速度也达15μm/h。
-
A total energy of > 5J , a focal spot size of order 100 μ m was demonstrated for target shots . It fulfills high-power requirements for laser-plasma interaction experiments .
通过模拟实验已经证实了该探针光的二倍频总能量大于5J,焦斑尺寸小于100μm,可以满足激光与等离子体相互作用的高功率要求。
-
An analysis of samples shows that , the matrix structures of the inside liner are martensite , retained austenite and eutectic carbide , with a hardness of 60 ~ 63HRC and a impact toughness of 7 ~ 7 5J / cm 2 ;