R ~ T and X ~ T relations of the sample were measured with the zero resistance temperature T_ ( C0 )≈ 91 K and the all diamagnetic temperature being 88K .
测量了样品的电阻与温度、磁化率与温度的关系,得到零电阻温度T(C0)≈91K,完全抗磁性温度88K。
-
Films on SrTiO_3 and ZrO_2 sub-strates have zero resistance at 88K and critical current density of 8 × 10 ~ 5A / cm ~ 2 ( 77K ) .
生长在SrTiO3和ZrO2衬底上的薄膜零电阻温度88K,77K零场临界电流密度Jc(?)