  1. Friction coefficient decreased with the increasing sliding speed and diameter of stainless steel ball . It reduced 54.24 % , while the sliding speed enhancing from 45r / min to 225r / min.

    摩擦副的摩擦系数随滑动速度和不锈钢球直径的增加而下降,当滑动速度从45r/min升至225r/min时,摩擦副的摩擦系数下降54.24%;

  2. Furthermore , reaction temperature and screw rotate speed have great effect on grafting polymerization . The study result shows that the high performance polymer with high grafting rate can be obtained at the 170 ~ 190 ℃ and rotate speed is 30 ~ 45r / min.